Nickel-chromium alloy
Manganin Constantan copper alloy
Cu-Ni alloy
Nichrome Precision alloy
Pure Nickel alloy
Nickel-aluminium(wireNi-A) alloy
Monel alloy
Hastelley alloy
Inconel alloy
Fe-Cr-Al alloy
Featured products
Alibaba Guaranteed
nickel alloy flat strip nichrome high resistance tape cr20ni30 electric heating resistance
$15.00 - $17.00
Shipping to be negotiated
Min. Order: 20 kilograms
High Temperature
High temperature resistance heating Alloy Cr20Ni80 bar
$15.00
Shipping to be negotiated
Min. Order: 500 kilograms
Best Price Hastelly Alloys C-276 Drill Bit Wire
$32.00 - $40.00
Shipping to be negotiated
Min. Order: 50 kilograms
Factory Price Nickel Chrome Flat wire Cr20Ni35 Heat Resistance Nichrome Wire for Heat Sealer Machine
$14.00 - $16.00
Shipping to be negotiated
Min. Order: 20 kilograms
Factory Hot Sale Pure Nickel Monel Flat Strip 400 K500 Best Price Guaranteed
$40.00
Shipping to be negotiated
Min. Order: 100 kilograms
FeCrAl Alloy Electric Resistance Wire 0Cr13Al4 0Cr15Al5 0Cr19Al2 0Cr21Al4 0Cr21Al6 0Cr25Al5 0Cr21Al6Nb 0Cr27Al7Mo2
$5.00 - $7.00
Shipping to be negotiated
Min. Order: 2 kilograms
High Quality Hastelly C-276 B-2 B-3 C-4 C-22 Flange & Rin Drill Bit
$32.00 - $40.00
Shipping to be negotiated
Min. Order: 50 kilograms
High Quality Hastelly Alloy C-276 B-2 B-3 C-4 C-22 Drill Bit for Wire & Welding
$32.00 - $40.00
Shipping to be negotiated
Min. Order: 50 kilograms
Pure Nickel Strip
Best Price Pure nickel strip N6 N4 Ni200 Ni201 ASTM B126 B164
$25.00 - $27.00
Shipping to be negotiated
Min. Order: 50 kilograms
Manganin constantan alloy wire 6J12 6J8 6J13 6J40 CuMn7SN CuMn30Ni5
$22.00 - $30.00
Shipping to be negotiated
Min. Order: 50 kilograms
Lowest price Ni 60 nichrome alloy Cr15Ni60 Ni60 wire manufacturer
$18.00 - $20.00
Shipping to be negotiated
Min. Order: 20 kilograms
0Cr13Al4 Fe-Cr-AI Alloys Flat Strip Cemented Carbide for Drill Bit Use
$8.00 - $10.00
Shipping to be negotiated
Min. Order: 50 kilograms
High Quality Hastelly C-276 B-2 B-3 C-4 C-22 Flat Strip Drill Bit
$32.00 - $40.00
Shipping to be negotiated
Min. Order: 50 kilograms
Best Price Nickel Alloy Hastelloy Alloy C276 C22 B B2 B3 B-2 B-3 Flag&Ring
$31.00 - $32.00
Shipping to be negotiated
Min. Order: 50 kilograms
Nichrome Precision Alloys Wire Drill Bit 1J330 1J331 1J332 1J335 1J350 1J479 1J485 4J332 4J332A 4J328 4J329 4J336 4J342 4J343
$23.00 - $40.00
Shipping to be negotiated
Min. Order: 50 kilograms
Monel Alloys Wire Drill Bit Type Monel 400 R405 K500 502
$23.00 - $35.00
Shipping to be negotiated
Min. Order: 50 kilograms